Molecular-Dynamics Simulations on Nanoindentation of Graphene-Diamond Composite Superstructures in Interlayer-Bonded Twisted Bilayer Graphene: Implications for Mechanical Metamaterials
- Citation:
- Chen, M, Weerasinghe A, Muniz AR, Ramasubramaniam A, Maroudas D.
2021. Molecular-Dynamics Simulations on Nanoindentation of Graphene-Diamond Composite Superstructures in Interlayer-Bonded Twisted Bilayer Graphene: Implications for Mechanical Metamaterials. ACS Applied Nano Materials. 4:8611-8625.